Features
Tech Specs
Single-channel voltage range: 100V to 1500V
Current range: 200A to 1600A (customizable).
Supports parallel operation of up to 4 channels (pulse/simulation testing unavailable in parallel mode), enabling seamless testing for energy storage Packs, ultra-high-voltage battery clusters, and high-voltage DC source simulation testing (PCS testing).

AC/DC and DC/DC dual-stage high-frequency isolated modular architecture enhances system scalability and flexibility, ensuring efficient production and maintenance.

Supports free switching between constant current, constant voltage, and constant power charge/discharge modes. With built-in pulse steps, condition simulation, and continuous charge/discharge switching functions, it meets testing needs such as battery cycle life and condition reproduction.
Cycle Life Testing / Pulse Testing / Condition Simulation / DCIR Test
Voltage & Current Accuracy: ±0.02% F.S.
Current Response Time: ≤10ms
Current Switching Time: ≤20ms
Minimum Pulse Width: 100ms

Multi-protocol communication interfaces: supports TCP/IP Ethernet, CAN FD/CAN/RS485, and mainstream BMS systems, enabling real-time data interaction and remote monitoring.
Peripheral synergy: integrates with water chillers, high/low-temperature environmental chambers, vibration testers, and other equipment to build a unified testing platform. Simulates complex operating conditions (e.g., high/low-temperature charge/discharge, vibration-based performance validation).

Precision data acquisition & logging: 24-bit high-resolution voltage/current sampling with a minimum recording interval of 10ms (100ms for auxiliary channels). Centralized MySQL database management ensures traceability across millions of test data entries.
Intelligent analysis & visualization: supports Excel/TXT data export and features built-in DCIR (Direct Current Internal Resistance) testing functionality for rapid report generation, boosting R&D efficiency.

| Equipment name | 3000V Ultra-High Voltage Battery Testing System |
|---|---|
| Model | CE-6001n-3000V200A |
| Voltage | |
| Output range | Charge:0V~3000V
Discharge :100V~3000V |
| Min discharge voltage | 100V |
| Accuracy | ±0.02% of F.S. |
| Resolution | 24bit |
| Current | |
| Output range | 1A~200A |
| Accuracy (independent range) | 0.02% of F.S. |
| CV cut-off current | 0.05% of F.S.(Each independent range) |
| Resolution | 24bit |
| Power | |
| Single channel output power | 300kW |
| Whole machine output power | 600kW |
| Time | |
| Current response time | ≤10ms |
| Current conversion time | ≤20ms |

Voltage & Current Accuracy: ±0.01% F.S.
Recording Frequency: 1000Hz
Current Response Time: ≤20μs
CV Testing
Type-C Power Port
6-Range Current Measurement

Voltage & Current Accuracy: ±0.02% F.S.
High-Frequency Sampling: 1000Hz
Current Conversion Time: ≤2ms
Current Response Time: ≤1ms
Minimum Pulse Width: 10ms
Feedback Efficiency (Max): 75%

Voltage & Current Accuracy: ±0.05% F.S.
Recording Frequency: 10Hz
Sampling Time: 100ms
Current Response Time: ≤1ms
Energy Efficiency: >65%
Off-Line Test: 1GB

Voltage & Current Accuracy: ±0.05% F.S.
Recording Frequency: 10Hz
Sampling Time: 100ms
Current Response Time: ≤1ms
Energy Efficiency: >65%
Off-Line Test: 1GB

Voltage & Current Accuracy: ±0.01% F.S.
Recording Frequency: 10Hz
Sampling Time: 100ms
Current Response Time: ≤500μs
Minimum Pulse Width: 500ms
Off-Line Test: 1GB

Volume: 100L
Space for Test System: 5U
Temperature Fluctuation: ≤0.9℉ (0.5℃)
Temperature Deviation: ±3.6℉ (±2℃)
Heating Time: 68°F ~ 302°F≤60min
(20℃ ~ 150℃≤60min)
Cooling Time: 68°F ~ -94°F≤75min
(20℃ ~ -70℃≤75min)

Volume: 100L*2
Number of Channels: 160CH
Temperature Fluctuation: ≤1.8℉ (1℃)
Temperature Deviation: ±3.6℉ (±2℃)
Heating Time: 77°F ~ 140°F≤30min
(25℃ ~ 60℃≤30min)
Cooling Time: 77°F ~ 32°F≤50min
(25℃ ~ 0℃≤50min)

Volume: 200L
Number of Channels: 160CH
Temperature Fluctuation: ≤1.8℉ (1℃)
Temperature Deviation: ±3.6℉ (±2℃)
Heating Efficiency: 77℉ ~ 140℉≤30min
(25℃ ~ 60℃≤30min)
Cooling Efficiency: 77℉ ~ 32℉≤50min
(25℃ ~ 0 ℃≤50min)