Features

Tech Specs

Resources

Dual-function integration of environmental simulation and performance testing 

This system combines a high-low temperature test chamber with a battery charge-discharge unit, covering a broad temperature range of -20°C to 85°C to simulate extreme conditions. Synchronized temperature and charge-discharge testing are managed through upper-computer software, meeting diverse requirements for battery R&D and quality inspection. 

NEWARE Desktop High-Low Temperature All-in-One Test Chamber-11

Key Specifications 

  • Current & voltage accuracy: ±0.02% F.S.

  • Sampling time: 100ms

  • Temperature range & deviation: -4°F ~ 185°F ±3.6°F(-20℃ ~ 85℃±2℃) 

  • Channel number: 16CH

  • Heating time: 68°F→185°F ≤30 min (20℃→85℃ ≤30 min, no load, average non-linear)

  • Cooling time: 68°F→-4°F ≤45 min (20℃→-20℃ ≤45 min, no load, average non-linear)

Mastering diversity, simplifying complexity 

By integrating the functions of compatible charging and discharging detection equipment and high and low temperature environmental test boxes into a meticulously designed solution, our products maximize space utilization and enhance equipment efficiency. Applicable for material research and button cell battery testing; the double-layer fixture tray design can securely accommodate up to 16 battery cells, providing a reliable and efficient solution for battery organization and management.

NEWARE Desktop High-Low Temperature All-in-One Test Chamber-001

Multiple safety protection mechanisms 

Emergency protection mechanisms such as power failure data recovery, short circuit protection, and fan abnormality detection are provided to prevent equipment damage.

NEWARE Desktop High-Low Temperature All-in-One Test Chamber-003

Technical Specifications

Equipment name High-Low Temperature Mini All-in-One Testing System
Model WGDW-20L-20C-220V-2U
Voltage 5V
Current 100mA
Temperature Range -4°F ~ 185°F ±3.6°F(-20℃ ~ 85℃±2℃)
Heating Time 68°F→185°F ≤30 min (20℃→85℃ ≤30 min, no load, average non-linear)
Cooling Time 68°F→-4°F ≤45 min (20℃→-20℃ ≤45 min, no load, average non-linear)
Temperature Fluctuation ≤±0.9°F (≤±0.5℃)
Temperature Deviation ±3.6°F (±2℃)
Nominal Content Volume 20L
Product Dimensions W17.3"×D21.7"×H20.7" (W440mm×D550mm×H525mm)

Want to explore further?
Download NEWARE product technical specifications for more details.

Download

Auxilaries and Optional Accessories

To support these high-precision measurement tools, we offer a wide range of product accessories.

Electrochemical Instruments

We offer powerful battery test equipments, environmental test chambers to provide comprehensive testing support for battery testing.

CT-8002S-5V100mA-CV-thumb

Battery Test Equipment-NEWARE

CT-8002S-5V100mA-CV

Portable Battery Testing System

  • Voltage & Current Accuracy: ±0.01% F.S.

  • Recording Frequency: 1000Hz

  • Current Response Time: ≤20μs 

  • CV Testing 

  • Type-C Power Port 

  • 6-Range Current Measurement

CE-6004-Pro-5V600A-thumb

Battery Test Equipment-NEWARE

CE-6006-Pro-6V1200A

CE-6000-Pro Power Cell Testing System

  • Voltage & Current Accuracy: ±0.02% F.S.

  • High-Frequency Sampling: 1000Hz 

  • Current Conversion Time: ≤2ms

  • Current Response Time: ≤1ms

  • Minimum Pulse Width: 10ms

  • Feedback Efficiency (Max): 75%

CE-4008Q-5V30A-thumb

Battery Test Equipment-NEWARE

CE-4008Q-5V30A

CE-4000 Battery Testing System

  • Voltage & Current Accuracy: ±0.05% F.S.

  • Recording Frequency: 10Hz

  • Sampling Time: 100ms

  • Current Response Time: ≤1ms

  • Energy Efficiency: >65%

  • Off-Line Test: 1GB

CE-4008Q-5V15A-thumb

Battery Test Equipment-NEWARE

CE-4008Q-5V15A

CE-4000 Battery Testing System

  • Voltage & Current Accuracy: ±0.05% F.S.

  • Recording Frequency: 10Hz

  • Sampling Time: 100ms

  • Current Response Time: ≤1ms

  • Energy Efficiency: >65%

  • Off-Line Test: 1GB

NEWARE-Battery Tester-CT-4008Q-5V100mA-124

Battery Test Equipment-NEWARE

CT-4008Q-5V100mA-124

CT-4000 Battery Testing System

  • Voltage & Current Accuracy: ±0.01% F.S.

  • Recording Frequency: 10Hz

  • Sampling Time: 100ms

  • Current Response Time: ≤500μs

  • Minimum Pulse Width: 500ms

  • Off-Line Test: 1GB

WGDW-100L-70C-380V-5U-thumb

NEWARE-Environmental Test Chamber

WGDW-100L-70C-380V-5U

High and Low Temperature All-in-One Testing System

  • Volume: 100L

  • Space for Test System: 5U

  • Temperature Fluctuation: ≤0.9℉ (0.5℃) 

  • Temperature Deviation: ±3.6℉ (±2℃)

  • Heating Time: 68°F ~ 302°F≤60min 

    (20℃ ~ 150℃≤60min) 

  • Cooling Time: 68°F ~ -94°F≤75min

    (20℃ ~ -70℃≤75min) 

NEWARE PC Coin Cell All-in-One Testing System

NEWARE-Environmental Test Chamber

WHW-200L2-0C-220V-9U-PC

PC All-in-One Battery Testing System

  • Volume: 100L*2

  • Number of Channels: 160CH

  • Temperature Fluctuation: ≤1.8℉ (1℃) 

  • Temperature Deviation: ±3.6℉ (±2℃)

  • Heating Time: 77°F ~ 140°F≤30min

    (25℃ ~ 60℃≤30min) 

  • Cooling Time: 77°F ~ 32°F≤50min

    (25℃ ~ 0℃≤50min)

NEWARE-Battery Tester-All-in-One Testing System-WIHW-200L-160CH-B

NEWARE-Environmental Test Chamber

WHW-200L-0C-220V-5V100mA-160CH

Coin Cell All-in-One Battery Testing System

  • Volume: 200L

  • Number of Channels: 160CH

  • Temperature Fluctuation: ≤1.8℉ (1℃) 

  • Temperature Deviation: ±3.6℉ (±2℃)

  • Heating Efficiency: 77℉ ~ 140℉≤30min

    (25℃ ~ 60℃≤30min)

  • Cooling Efficiency: 77℉ ~ 32℉≤50min

    (25℃ ~ 0 ℃≤50min)

NEWARE and Cookies
We use cookies to personalize and improve your experience with our website. By continuing to browse the site you are agreeing to our use of cookies.