Why charging switches to constant voltage at the voltage limit
Constant-current/constant-voltage charging is commonly abbreviated as CC-CV. During the constant-current (CC) stage, the battery receives charge at a specified current. The constant-voltage (CV) stage addresses a different condition: terminal voltage has reached its upper limit, but the battery can still accept additional charge. The charger therefore limits voltage and progressively reduces current as charging proceeds. [1]
Stopping at the voltage limit shortens the charging process but omits the charge that the subsequent CV stage could add. Maintaining the original constant current may instead drive terminal voltage above the limit. Switching to CV allows charging to continue while holding terminal voltage near the upper limit and reducing current until a termination condition is met. The transition therefore supports both voltage control and capacity utilization. [1]
Figure 1 plots voltage, current, and state of charge (SOC) against time. After the red voltage curve reaches 4.2 V and levels off, the blue current curve falls while the green SOC curve continues to rise. The key observation is that charge continues to accumulate even though voltage no longer increases. SOC in this figure is model-based; it illustrates the control behavior and does not replace a separate measurement of discharge capacity. [2]

Figure 1. Voltage, current, and SOC during CC-CV charging. SOC continues to rise during the CV stage. The original SOC scale from 0 to 1 is interpreted as normalized state of charge.
Reaching the voltage limit does not mean charging is complete
Terminal voltage during charging reflects the cell's state of charge as well as the ohmic voltage contribution and electrochemical polarization produced by current flow. With charging current defined as positive, a simplified expression is:
Vterm ≈ Ueq(SOC, T) + I RΩ + η
Here, T is temperature, RΩ is the equivalent ohmic resistance, and η represents polarization associated with interfacial reactions and nonuniform concentration distributions. This expression explains the voltage contributions; terminal voltage alone cannot determine the cell's internal state. A higher current raises terminal voltage during charging, so the voltage limit may be reached while substantial concentration gradients remain and further charge can still be accepted. [1]
As lithium ions continue to enter the electrodes, equilibrium voltage and internal concentration distributions continue to change. Under CV control, current is reduced so that the ohmic and polarization contributions occupy less of the available voltage margin. This allows charging to continue at a declining rate while respecting the terminal-voltage limit. Maintaining the original constant current could instead push the cell above that limit. [1]
The same ten minutes can add much less charge near the end
The amount of charge added per unit time depends on the actual current. Charging capacity Q is obtained by integrating current over time:
Q = ∫ I(t) dt
When current is expressed in amperes and time in hours, Q is expressed in ampere-hours. For example, an average current of 3 A for 10 minutes adds 0.5 Ah. At an average current of 0.3 A, the same 10 minutes adds only 0.05 Ah, a tenfold difference.
Integrating the stages separately gives the CC-stage charge QCC, the CV-stage charge QCV, and the total charge Qtotal = QCC + QCV. Compared with stopping when the voltage limit is first reached, continuing through the CV stage adds QCV. This is the most direct measure of the CV stage's contribution. Its share of total charge should be calculated from the measured curves rather than assigned a fixed percentage.
Additional charge input does not necessarily equal additional usable discharge capacity. To evaluate the CV stage's contribution to usable capacity, compare two otherwise equivalent tests: stop one charge at the end of CC, and continue the other through CV to the specified termination current. Then discharge both under the same rest time, temperature, current, and lower-voltage limit. The difference in measured discharge capacity shows how much usable capacity the extra charging time provides.
Figure 2 comes from Zhang's study of graphite/NCA coin full cells. NCA refers to the nickel-cobalt-aluminum oxide cathode. Cells were charged at different C-rates between 3.0 and 4.2 V, then discharged at a common rate of 0.5C. Red circles and blue triangles in the left panel show charge and discharge capacities, respectively. The right panel plots voltage against capacity. After a charge curve reaches 4.2 V, its horizontal segment continues to the right, showing the additional charge accepted during CV. [4]

Figure 2. Charge/discharge capacities and voltage-capacity curves at different charging rates. The left panel shows final capacities for each cycle. The horizontal segments at the top of the charge curves in the right panel correspond to the CV stage.
Follow one charge curve from left to right in the right panel: voltage first rises, then becomes constant at the limit while capacity continues to increase along the horizontal axis. The width of that horizontal segment is the charge added during CV. Because the colors represent different charging rates, differences between colored curves cannot be treated directly as the benefit of including versus omitting CV.
Charge termination depends on the specified cutoff conditions
CV charging does not require waiting indefinitely for current to reach zero. A common protocol ends charging when current falls to a specified threshold, with appropriate time and protection limits also applied. The termination current should follow the cell specification and test objective. Record both the threshold and the condition that actually ended the test.
With other conditions unchanged, a lower termination current generally extends the low-current tail and may increase both charging time and charge input. If two tests use different termination currents, their time and capacity differences cannot be attributed entirely to cell performance. At minimum, report charging current, upper-voltage limit, and termination current together.
An earlier current taper alone does not establish battery aging
After a period of use, the same cell may enter CV earlier than before. One possible reason is increased impedance: at the same charging current, larger ohmic and polarization contributions can make terminal voltage reach its limit before the same amount of charge has been added. Current then begins to taper, but this does not mean the battery has charged faster or stored more charge. [1,3]
The left panel of Figure 3 compares charging-voltage curves at different cycle numbers. Some later-cycle curves reach the 4.2 V plateau earlier, indicating a shorter CC stage. The right panel identifies the CC and CV durations and other time intervals. Xiao et al. used changes in these time features to analyze battery health. [3]

Figure 3. Charging-voltage curves at different cycle numbers. Later-cycle curves reach the 4.2 V plateau earlier in the left panel. The right panel identifies the charging stages and time intervals analyzed in the original study.
To determine whether capacity has declined, first standardize initial SOC, temperature, charging current, upper-voltage limit, and termination current. Compare the charging curves and perform discharge tests under the same conditions. If the cell enters CV earlier but its discharge capacity has not decreased, the earlier transition alone does not establish capacity fade. A sustained decrease in discharge capacity under standardized conditions provides direct evidence of capacity loss.
The distinction is between reaching the charging-voltage limit earlier, which describes charging behavior, and the amount of charge the battery can subsequently deliver, which describes usable capacity. Charging curves reveal changes in behavior; discharge-capacity measurements help determine whether those changes have affected storage capability.
Make charging-test results comparable
Start from a consistent initial condition. When comparing different cycle stages of the same cell or comparing different cells, apply defined preconditioning, discharge endpoints, rest periods, and temperature conditions. Different operating histories can shift charging curves even when the same charging program is used.
Next, fix charging current, upper-voltage limit, termination current, and data-recording settings. Retain voltage, current, temperature, and step records on a common time base. Separate the data at the CC-to-CV transition and calculate each stage's duration and charge input. In addition to total charging time, report the CV charge fraction QCV/(QCC + QCV) if useful. Compare this fraction under the same conditions rather than treating it as a universal health indicator.
If current decreases before voltage reaches its limit, first check the active test step, temperature-based current limits, power limits, and protection logs. If voltage has reached the limit, check whether the system has entered CV normally. When temperature or connections are suspected, change one condition at a time during repeat tests so that its effect can be identified.
Record the complete charging process with a NEWARE test system
The relevant charging steps in NEWARE BTS allow CC, CV, and termination conditions to be set according to the cell test protocol, with voltage, current, time, and capacity records available for analysis. Align the onset of current taper with terminal voltage and test-step status, then compare the charge contributed by the CC and CV stages. For temperature comparisons, use suitable environmental equipment and temperature-acquisition configurations, and retain cell-temperature records.
Select a test configuration that covers the cell's voltage and current ranges while meeting low-current measurement requirements during the CV tail. The recording interval should resolve step transitions and current changes rather than leave data too sparse to trace the transition. Available step names, measurement ranges, and temperature-acquisition capabilities depend on the equipment and software version.
Conclusion
Slower charging near full charge commonly reflects the normal current taper after the transition from CC to CV. Read voltage, current, and termination conditions together: has voltage reached its limit, how much charge does the tail add, and what condition ends the test? These observations provide a basis for assessing charging strategy, temperature effects, and aging, and for making meaningful comparisons.
References
[1] Tomaszewska A, Chu Z, Feng X, et al. Lithium-ion battery fast charging: A review. eTransportation, 2019, 1: 100011. https://doi.org/10.1016/j.etran.2019.100011
[2] Fenner G P, Stringini L W, Rangel C A S, Canha L N. Comprehensive Model for Real Battery Simulation Responsive to Variable Load. Energies, 2021, 14(11): 3209. https://doi.org/10.3390/en14113209
[3] Xiao B, Xiao B, Liu L. State of Health Estimation for Lithium-Ion Batteries Based on the Constant Current-Constant Voltage Charging Curve. Electronics, 2020, 9(8): 1279. https://doi.org/10.3390/electronics9081279
[4] Zhang S S. Identifying rate limitation and a guide to design of fast-charging Li-ion battery. InfoMat, 2020, 2(5): 942-949. https://doi.org/10.1002/inf2.12058