Modifying the Control Unit sampling frequency

Latest updated: Jan 02, 2024

1. To modify the sampling frequency of the Control Unit, you first need to obtain the Control Unit's IP address.

(1) You can find it on the physical label of the Control Unit.

(2) You can check it on the Control Unit's display screen.

(3) You can find it in the BTS software.

2. Follow these steps:

(1) Open a web browser and enter the Control Unit's IP address: 192.168.10.3.


(2) Access the Neware Equipment Management System and log in with the username "neware" and password "xinwei".


(3) Click on the 'Device Configuration' in the left sidebar, where you can modify the Control Unit's sampling frequency.


Note: Ensure that the Control Unit's sampling frequency is consistent with the Tester's sampling frequency.


neware-battery-test-newareAI neware-battery-test-newareStore neware-battery-test-neware-newell

Find the Right Battery Test Equipment for Your Needs.

Application Scenarios

Trusted testing solutions for global clients.

Solid-State Battery Research - NEWARE Solid-State Battery test
Solid-State Battery Research

The lab focuses on solid-state battery research to overcome traditional lithium batteries' safety and energy density issues, supporting environmental sustainability. It develops innovative solid-state electrolytes, refines electrode materials, and investigates ion transfer and interface stability to revolutionize battery technology.

View more
Electric Vehicle Battery
Electric Vehicle Battery

The electric vehicle battery industry is rapidly developing, focusing on technological innovation, market competition, and sustainability. Research hotspots include solid-state batteries, new types of electrolytes, BMS optimization, and recycling technologies. The environmental adaptability, safety, and economic viability of batteries are key research areas, and the industry is expected to undergo more innovation and transformation.

View more
Battery Materials Research - NEWARE battery test
Battery Materials Research

We specialize in battery preparation technology research, focusing on overcoming existing energy storage challenges by innovating in electrode materials, battery chemistry, and manufacturing processes to improve performance, enhance safety, and reduce costs. Sustainability and recycling technologies for batteries are also emphasized to mitigate environmental impacts and foster the growth of green energy.

View more
Energy Storage Battery Testing Solution
Energy Storage System

To power the energy transition, the storage industry is evolving towards large-scale, high-quality development, focusing on safety, efficiency, and lifecycle value over mere price competition.

View more
NEWARE and Cookies
We use cookies to personalize and improve your experience with our website. By continuing to browse the site you are agreeing to our use of cookies.