Features
Resources
The fine-tuning feature of the top voltage probe ensures a more uniform contact force, guaranteeing the accuracy of measurements. The overall 2.5kg spring force design provides a solid guarantee for continuous and stable data collection.
| Model | P103-12-TZ-LK-TDU-30A-Z-001 | P103-12-TZ-LK-TDU-30A-F-001 |
| Nut | M5 | M8 |
| Probe Length | 2.14″(54.3mm) | 1.28″(32.5mm) |
| Current | ≤30A | |
| Contact Resistance | ≤1mΩ | |
| Spring force | Voltage probe spring force: 200g, Overall spring force: 2.5kg | |
| Heat Resistant | 302℉(150℃) | |
| Fire Resistance Rating | V0 | |
Efficient cylindrical battery probes, designed for precise capacity sorting and internal resistance testing. They offer stable contact to ensure the accuracy and repeatability of test data, optimizing the assessment of battery performance.
The probe's internal resistance is less than 1mΩ, ensuring efficient and stable current transmission. The gold-plated surface treatment not only enhances conductivity but also improves corrosion resistance, ensuring reliability for long-term use.
The probe structure is designed to exceed 30,000 cycles of service life, demonstrating excellent durability. At the same time, it can withstand temperatures up to 150℃, ensuring performance is unaffected in extreme environments.

Voltage & Current Accuracy: ±0.01% F.S.
Recording Frequency: 1000Hz
Current Response Time: ≤20μs
CV Testing
Type-C Power Port
6-Range Current Measurement

Voltage & Current Accuracy: ±0.05% F.S.
Recording Frequency: 10Hz
Sampling Time: 100ms
Current Response Time: ≤1ms
Energy Efficiency: >65%
Off-Line Test: 1GB

Voltage & Current Accuracy: ±0.05% F.S.
Recording Frequency: 10Hz
Sampling Time: 100ms
Current Response Time: ≤1ms
Energy Efficiency: >65%
Off-Line Test: 1GB

Voltage & Current Accuracy: ±0.01% F.S.
Recording Frequency: 10Hz
Sampling Time: 100ms
Current Response Time: ≤1ms
Minimum Pulse Width: 500ms
Off-Line Test: 1GB

Volume: 100L
Space for Test System: 5U
Temperature Fluctuation: ≤0.9℉ (0.5℃)
Temperature Deviation: ±3.6℉ (±2℃)
Heating Time: 68°F ~ 302°F≤60min
(20℃ ~ 150℃≤60min)
Cooling Time: 68°F ~ -94°F≤75min
(20℃ ~ -70℃≤75min)

Volume: 100L*2
Number of Channels: 160CH
Temperature Fluctuation: ≤1.8℉ (1℃)
Temperature Deviation: ±3.6℉ (±2℃)
Heating Time: 77°F ~ 140°F≤30min
(25℃ ~ 60℃≤30min)
Cooling Time: 77°F ~ 32°F≤50min
(25℃ ~ 0℃≤50min)

Volume: 200L
Number of Channels: 160CH
Temperature Fluctuation: ≤1.8℉ (1℃)
Temperature Deviation: ±3.6℉ (±2℃)
Heating Efficiency: 77℉ ~ 140℉≤30min
(25℃ ~ 60℃≤30min)
Cooling Efficiency: 77℉ ~ 32℉≤50min
(25℃ ~ 0 ℃≤50min)

Volume: 25L
Number of Channels: 32CH
Temperature Fluctuation: ≤1.8℉ (1℃)
Temperature Deviation: ±3.6℉ (±2℃)
Heating Time: 77°F ~ 140°F≤50min
(25℃ ~ 60℃≤50min)
Cooling Time: 77°F ~ 59°F≤60min