With a voltage range of -5V~5V and six current ranges from 0.1μA to 100mA, it achieves ±0.01% of F.S. precision. Using 24bit AD sampling and four - wire connection technology, it ensures accurate capture of tiny signals. The dual - closed - loop control of constant current and voltage provides lab - level precision for battery material research.

Current Ranges: 0.1 mA, 1 mA, 5 mA, 10 mA, 50 mA, 100 mA

6-range switching, precision defined

Multiple test modes with enhanced CV testing. 

Comprehensive testing and data analysis: Features cycle life, rate charge-discharge, pulse simulation, GITT, DCIR, and dQ/dV differential capacity curve analysis. CV testing integration: Allows CV testing within charge-discharge cycles. Customize cycle numbers for automatic CV scans to simulate battery aging and analyze electrode reaction characteristics.

Multiple test modes with enhanced CV testing

Fast response and seamless current switching. 

It has a current response time of ≤20μs and can switch currents seamlessly. This allows it to quickly capture dynamic changes during battery charge/discharge, ensuring real - time and accurate data for reproducing true transient conditions.

Fast response and seamless current switching

Efficient data management and comprehensive safety assurance.

Test data is centrally stored in a MySQL database and can be exported in various formats such as Excel, TXT, and CSV for easy analysis and report generation, enhancing R&D efficiency. Dual software-hardware protection mechanisms, including voltage/current limits, temperature monitoring, and reverse connection prevention, along with power-loss data recovery and offline testing support, ensure equipment and battery safety.

Technical Specifications

Equipment name CT-8000 Battery Testing System
Model CT-8008S-5V100mA-CV
Resolution AD:24bit;DA:16bit
Voltage
Output range -5V-5V
Min discharge voltage -5V
Accuracy ± 0.01% of F.S.
Stability 0.02% of F.S.
Current
Output range Range1: 0.1mA; Range2: 1mA; Range3: 5mA; Range4: 10mA; Range5: 50mA; Range6: 100mA
Accuracy ± 0.01% of F.S.
Stability 0.02% of F.S.
Power
Single channel output power 0.5W
Accuracy ±0.02% of F.S.
Stability 0.04% of F.S.

Want to explore further?
Download NEWARE product technical specifications for more details.

Download

Auxilaries and Optional Accessories

To support these high-precision measurement tools, we offer a wide range of product accessories..

Electrochemical Instruments

We offer powerful battery test equipments, environmental test chambers to provide comprehensive testing support for battery testings.

CT-8002S-5V100mA-CV-thumb

Battery Test Equipment-NEWARE

CT-8002S-5V100mA-CV

Portable Battery Testing System

  • Voltage & Current Accuracy: ±0.01% F.S.

  • Recording Frequency: 1000Hz

  • Current Response Time: ≤20μs 

  • CV Testing 

  • Type-C Power Port 

  • 6-Range Current Measurement

CE-6004-Pro-5V600A-thumb

Battery Test Equipment-NEWARE

CE-6006-Pro-6V1200A

CE-6000-Pro Power Cell Testing System

  • Voltage & Current Accuracy: ±0.02% F.S.

  • High-Frequency Sampling: 200Hz 

  • Current Conversion Time: ≤2ms

  • Current Response Time: ≤1ms

  • Minimum Pulse Width: 10ms

  • Feedback Efficiency (Max): 75%

CE-4008Q-5V30A-thumb

Battery Test Equipment-NEWARE

CE-4008Q-5V30A

CE-4000 Battery Testing System

  • Voltage & Current Accuracy: ±0.05% F.S.

  • Recording Frequency: 10Hz

  • Sampling Time: 100ms

  • Current Response Time: ≤1ms

  • Energy Efficiency: >65%

  • Off-Line Test: 1GB

CE-4008Q-5V15A-thumb

Battery Test Equipment-NEWARE

CE-4008Q-5V15A

CE-4000 Battery Testing System

  • Voltage & Current Accuracy: ±0.05% F.S.

  • Recording Frequency: 10Hz

  • Sampling Time: 100ms

  • Current Response Time: ≤1ms

  • Energy Efficiency: >65%

  • Off-Line Test: 1GB

NEWARE-Battery Tester-CT-4008Q-5V100mA-124

Battery Test Equipment-NEWARE

CT-4008Q-5V100mA-124

CT-4000 Battery Testing System

  • Voltage & Current Accuracy: ±0.01% F.S.

  • Recording Frequency: 10Hz

  • Sampling Time: 100ms

  • Current Response Time: ≤500μs

  • Minimum Pulse Width: 500ms

  • Off-Line Test: 1GB

WGDW-100L-70C-380V-5U-thumb

NEWARE-Environmental Test Chamber

WGDW-100L-70C-380V-5U

High and Low Temperature All-in-One Testing System

  • Volume: 100L

  • Space for Test System: 5U

  • Temperature Fluctuation: ≤0.9℉ (0.5℃) 

  • Temperature Deviation: ±3.6℉ (±2℃)

  • Heating Time: 68°F ~ 302°F≤60min 

    (20℃ ~ 150℃≤60min) 

  • Cooling Time: 68°F ~ -94°F≤75min

    (20℃ ~ -70℃≤75min) 

NEWARE PC Coin Cell All-in-One Testing System

NEWARE-Environmental Test Chamber

WHW-200L2-0C-220V-9U-PC

PC All-in-One Battery Testing System

  • Volume: 100L*2

  • Number of Channels: 160CH

  • Temperature Fluctuation: ≤1.8℉ (1℃) 

  • Temperature Deviation: ±3.6℉ (±2℃)

  • Heating Time: 77°F ~ 140°F≤30min

    (25℃ ~ 60℃≤30min) 

  • Cooling Time: 77°F ~ 32°F≤50min

    (25℃ ~ 0℃≤50min)

NEWARE-Battery Tester-All-in-One Testing System-WIHW-200L-160CH-B

NEWARE-Environmental Test Chamber

WHW-200L-0C-220V-5V100mA-160CH

Coin Cell All-in-One Battery Testing System

  • Volume: 200L

  • Number of Channels: 160CH

  • Temperature Fluctuation: ≤1.8℉ (1℃) 

  • Temperature Deviation: ±3.6℉ (±2℃)

  • Heating Efficiency: 77℉ ~ 140℉≤30min

    (25℃ ~ 60℃≤30min)

  • Cooling Efficiency: 77℉ ~ 32℉≤50min

    (25℃ ~ 0 ℃≤50min)

NEWARE and Cookies
We use cookies to personalize and improve your experience with our website. By continuing to browse the site you are agreeing to our use of cookies.