Features
Tech Specs
Resources
Smart auto-switching of 6 current ranges, ±0.02% of F.S. current precision, delivers mA-level current for 3C battery standby power testing and high-current pulses for fast-charging protocol tests. 7-Mode Flexibility: Supports 7 modes like CC/CV/CP/CR/pulse charge-discharge, covering the full-life-cycle of batteries. Its minimum pulse width of 20ms and support for 32-pulse continuous switching per step aid accurate DCIR calculation.

Rapid 500μs response, with current rise time ≤500μs (10%~90% of F.S.) and charge-discharge switching ≤1ms (–90%~90% of F.S.), boosts test efficiency for high-dynamic testing.
It has a >70% energy-efficient design. Using green energy-saving tech, it cuts energy use, meets sustainable-lab standards, and supports low-carbon testing.

Dual-loop control technology: independent dual - loop structure for CV and CC sources ensures fast response and strong stability (0.04% of F.S. voltage stability).
4-wire connection: eliminates line-loss errors for precise voltage and current sampling.
Multiple safety protections: features over-voltage/current/protection, reverse connection protection, over-temperature protection, emergency stop, IP20 rating to ensure device and personnel safety.
Industrial-grade communication interfaces: equipped with standard TCP/IP and optional CAN, RS485 for BMS communication, supporting DBC configuration for seamless BMS integration.
Professional data management: centralized data management via MySQL databases for efficient, secure storage and retrieval.

Each single step can run for up to 365×24 hours, meeting long - term aging test needs. The equipment maintains accuracy in a wide temperature range of 0~40°C, with a storage temperature range of -10~50°C, making it suitable for labs. It also ensures a quiet test environment with noise levels below 75dB at a distance of 1m.

| Equipment name | CE-8000 Battery Testing System |
|---|---|
| Model | CT-8008S-5V30A |
| Resolution | AD:24bit;DA:16bit |
| Voltage | |
| Output range | 0V-5V |
| Min discharge voltage | 1V |
| Accuracy | ± 0.02% of F.S. |
| Current | |
| Output range | Range1: 300mA, Range2: 1A, Range3: 3A Range4: 6A, Range5: 12A, Range6: 30A |
| Accuracy | ± 0.02% of F.S. |
| Power | |
| Single channel output power | 150W |
| Accuracy | ±0.04% of F.S. |
| Time | |
| Current conversion time | ≤1ms (-90% ~ 90% of F.S.) |
| Data acquisition rate | 1000Hz |

Voltage & Current Accuracy: ±0.01% F.S.
Recording Frequency: 1000Hz
Current Response Time: ≤20μs
CV Testing
Type-C Power Port
6-Range Current Measurement

Voltage & Current Accuracy: ±0.02% F.S.
High-Frequency Sampling: 1000Hz
Current Conversion Time: ≤2ms
Current Response Time: ≤1ms
Minimum Pulse Width: 10ms
Feedback Efficiency (Max): 75%

Voltage & Current Accuracy: ±0.05% F.S.
Recording Frequency: 10Hz
Sampling Time: 100ms
Current Response Time: ≤1ms
Energy Efficiency: >65%
Off-Line Test: 1GB

Voltage & Current Accuracy: ±0.05% F.S.
Recording Frequency: 10Hz
Sampling Time: 100ms
Current Response Time: ≤1ms
Energy Efficiency: >65%
Off-Line Test: 1GB

Voltage & Current Accuracy: ±0.01% F.S.
Recording Frequency: 10Hz
Sampling Time: 100ms
Current Response Time: ≤500μs
Minimum Pulse Width: 500ms
Off-Line Test: 1GB

Volume: 100L
Space for Test System: 5U
Temperature Fluctuation: ≤0.9℉ (0.5℃)
Temperature Deviation: ±3.6℉ (±2℃)
Heating Time: 68°F ~ 302°F≤60min
(20℃ ~ 150℃≤60min)
Cooling Time: 68°F ~ -94°F≤75min
(20℃ ~ -70℃≤75min)

Volume: 100L*2
Number of Channels: 160CH
Temperature Fluctuation: ≤1.8℉ (1℃)
Temperature Deviation: ±3.6℉ (±2℃)
Heating Time: 77°F ~ 140°F≤30min
(25℃ ~ 60℃≤30min)
Cooling Time: 77°F ~ 32°F≤50min
(25℃ ~ 0℃≤50min)

Volume: 200L
Number of Channels: 160CH
Temperature Fluctuation: ≤1.8℉ (1℃)
Temperature Deviation: ±3.6℉ (±2℃)
Heating Efficiency: 77℉ ~ 140℉≤30min
(25℃ ~ 60℃≤30min)
Cooling Efficiency: 77℉ ~ 32℉≤50min
(25℃ ~ 0 ℃≤50min)