Table of Contents

    Cooperation Case

    NEWARE Cooperation Case: NEWARE Battery Tester to Help Battery Materials Research

    Latest updated: April 02, 2024

    Stalling oxygen evolution in high-voltage cathodes by lanthurization

    Stalling oxygen evolution in high-voltage cathodes by lanthurization

    High energy density has become a crucial factor in the future development of batteries. One key aspect is the development of high-voltage cathode materials. However, during high-voltage operation, cathode materials face challenges such as crystal structure degradation (e.g., lattice oxygen release), electrolyte decomposition leading to battery failure, and safety issues like thermal runaway. Taking lithium cobalt oxide cathode as an example, serious structural degradation and oxygen release occur when the upper voltage limit is increased from 4.2 V to 4.6 V.

    A team led by Fuqiang Huang from Peking University and Ju Li from MIT, among others, conducted a systematic analysis of the oxygen evolution issue in high-voltage layered cathode materials. They proposed a universal strategy to significantly improve the high-voltage stability of layered cathode materials. This strategy is based on controllable liquid-phase ion exchange reactions, which not only achieve high uniformity of coating but also enhance the ion bonding between transition metals and oxygen. It inhibits the migration of reactive oxygen to the surface. The strategy demonstrates good universality and can be applied to all layered oxide cathodes, enabling large-scale production. It provides a new approach for the industrialization of high-voltage ternary nickel-rich cathodes and lithium-rich manganese-based cathodes. This work was published in the top-tier journal Nature Energy, with Mingzhi Cai and Yanhao Dong as co-first authors.

    NEWARE battery test system

    The NEWARE-CT-4008Tn-battery tester helps study and test dQdV differential capacity curves

    In this academic paper, all electrochemical tests were performed using the NEWARE Battery Test System (CT-4008Q-5V100mA-124). This testing system is powerful, capable of conducting dQ/dV differential capacity curve measurements to help researchers understand different electrochemical reactions. It also enables customization of test conditions and segmented recording, catering to diverse battery testing requirements.

    NEWARE is one of the world's leading battery testing companies, offering a comprehensive range of battery testers, battery testing solutions, and battery production services. NEWARE also provides BTS host computer integration with temperature chamber control and integrated constant temperature chambers. Whether you are a battery manufacturer or involved in battery testing-related research, NEWARE is your best choice.


    neware-battery-test-newareAI neware-battery-test-newareStore neware-battery-test-neware-newell

    A Complete Validation Solution

    Every piece of the puzzle, engineered to work in concert.

    View all

    Still can't find your answer?

    Our application engineers are ready to help with technical issues, calibration requests, and custom testing solutions.
    Name
    Country
    City Name
    Company Name
    Phone Number
    Email Address *
    Products
    Model
    Detailed Request
    NEWARE and Cookies
    We use cookies to personalize and improve your experience with our website. By continuing to browse the site you are agreeing to our use of cookies.