Auxiliary channel introduction and wiring guide

Latest updated: Apr 10, 2026

1. What is an Auxiliary Channel?

The NEWARE Auxiliary Channel is used together with charge-discharge equipment to measure the voltage and temperature of single cells or battery packs. Early auxiliary channels came in the following models:

  • CA-4008-1U-VT: for first-generation 4-series equipment;

  • CA-4008-1U-VT-18P: thermistor, for 4-series equipment;

  • CA-4008-1U-VT-EVT: thermistor, for 7-series high-voltage equipment;

  • CA-4008-1U-VT-KX: Type-K thermocouple, for 4-series equipment;

  • CA-4008-1U-VT-TX: Type-T thermocouple, for 4-series equipment;

  • CA-5008-1U-VT: for 3008N, 5-series and 9-series equipment;

The latest auxiliary-channel model is CA-4008n-1U-5VT-TC-DB25, which supports both 110 V and 220 V supply voltages.

Auxiliary Channel

Figure 1


2. Auxiliary Channels Introduction

Take the CA-4008n-1U-5VT-TC-DB25 as an example: the left side is the auxiliary channel voltage-sampling port, and the right side is the auxiliary channel temperature-sampling port.

 1 (2)

Figure 2


3. How to Cable the Auxiliary Channel

First, connect the control unit, auxiliary channel, and tester in sequence with power cables, then link them together in series using network cables.

3

Figure 3


4. Using Auxiliary Channels in BTS Software

4.1 Channel Mapping  

Select the main channel, right-click and choose "Reset Mapping".

4

Figure 4


Then right-click again and choose "Auxiliary Channel Default Mapping".

5

Figure 5


After the mapping is executed, the auxiliary channels on the left will turn gray.

6

Figure 6


4.2 Average Mapping

Average mapping distributes all auxiliary channels evenly under each main channel.  

For example, if the unit has 8 auxiliary channels and 8 main channels, each main channel will show one auxiliary channel after the mapping is executed.

7

Figure 7


4.3 Priority Mapping

After priority mapping is executed, all auxiliary channels will be mapped under the first main channel on the page.

8

Figure 8


4.4 Custom Mapping

You can set the number of auxiliary channels mapped to each main channel, or drag and drop auxiliary channels to map them manually.

 9

Figure 9


Once mapping is complete, right-click to save the mapping. Return to the main page to view the auxiliary channels (displaying voltage and temperature values).

Figure 10 


5. Data Collection with BTSDA Software

Right-click to view “Channel Data” and enter the BTSDA page. Right-click and select “Parameter Settings” to configure “Cell Voltage/Temperature”.

Figure 11


12

Figure 12


Click the “+” in the data table to expand the record-level data. Voltage and temperature for each auxiliary channel are recorded and collected at the specified time intervals.

13

Figure 13


Click the green button at the top of the page to export data as needed.

14

Figure 14



neware-battery-test-newareAI neware-battery-test-newareStore neware-battery-test-neware-newell

Find the Right Battery Test Equipment for Your Needs.

Application Scenarios

Trusted testing solutions for global clients.

Solid-State Battery Research - NEWARE Solid-State Battery test
Solid-State Battery Research

The lab focuses on solid-state battery research to overcome traditional lithium batteries' safety and energy density issues, supporting environmental sustainability. It develops innovative solid-state electrolytes, refines electrode materials, and investigates ion transfer and interface stability to revolutionize battery technology.

View more
Electric Vehicle Battery
Electric Vehicle Battery

The electric vehicle battery industry is rapidly developing, focusing on technological innovation, market competition, and sustainability. Research hotspots include solid-state batteries, new types of electrolytes, BMS optimization, and recycling technologies. The environmental adaptability, safety, and economic viability of batteries are key research areas, and the industry is expected to undergo more innovation and transformation.

View more
Battery Materials Research - NEWARE battery test
Battery Materials Research

We specialize in battery preparation technology research, focusing on overcoming existing energy storage challenges by innovating in electrode materials, battery chemistry, and manufacturing processes to improve performance, enhance safety, and reduce costs. Sustainability and recycling technologies for batteries are also emphasized to mitigate environmental impacts and foster the growth of green energy.

View more
Energy Storage Battery Testing Solution
Energy Storage System

To power the energy transition, the storage industry is evolving towards large-scale, high-quality development, focusing on safety, efficiency, and lifecycle value over mere price competition.

View more
NEWARE and Cookies
We use cookies to personalize and improve your experience with our website. By continuing to browse the site you are agreeing to our use of cookies.