Features
Tech Specs
Resources
Stable performance parameters to ensure accurate and reliable test data. At the same time, the product adopts modular design with each unit having 2 channels, which can be independently data acquisition.
Voltage & Current | Range1 | Range2 | Range3 | Range4 |
5V100mA | 0.2μA ~ 0.1mA | 0.1mA ~ 1mA | 1mA ~ 10mA | 10mA ~ 100mA |
*Other models can be customized according to voltage and current requirements.
4 current ranges from 0.5μA ~ 0.1mA, 0.1mA ~ 1mA, 1mA ~ 10mA , 10mA ~100mA can be selected to realize the controllable accuracy of small current in small range.
● Discharge Data Protection
● Offline Testing Function
● Voltage Upper Limit Setting
● Voltage Lower Limit Setting
● Current Upper Limit Setting
● Current Lower Limit Setting
● Capacity Upper Limit Setting
● Delay Time Setting
Delicate measurements at μA-level current, uncovering the essence of testing.
Based on NEWARE 5th generation test system architecture, it can perform Cycle Life Test, Rate Charging / Discharging Test, Pulse Simulation Test, HPPC, etc. Meanwhile, it can simulate the actual driving road conditions of electric vehicles by dynamic power or current waveform.
Tailored for advanced battery testing: enabling dQ/dV differential capacity curve analysis capability.
The software is fully functional, covering a variety of work-step settings, recording, and data storage to meet a wide range of testing needs.
Integrated peripheral devices such as Auxiliary Voltage, Auxiliary Temperature, and Environmental TestChambers for comprehensive testing and evaluation, providing multi-dimensional and quantifiable support for battery mass production testing.
Equipment name | CT-8000 Battery Testing System |
---|---|
Input power supply | AC 220V ±10% / 50Hz |
Input power | 25 W |
Resolution ratio | AD:24bit;DA:16bit |
Input impedence | ≥1GΩ |
Voltage | |
Voltage range per channel | 10mV~5V |
Minimum discharge voltage | -5 V |
Accuracy | ± 0.01% of F.S. |
Stability | ± 0.01% of F.S. |
Current | |
Current range per channel | Range 1:0.1 mA; Range 2:1 mA; Range 3:10 mA; Range 4:100 mA |
Accuracy | ± 0.02% of F.S. |
Constant pressure cut-off current | Range 1: 0.1 μA; Range 2: 1 μA; Range 3: 10 μA; Range 4: 100 μA |
Stability | ± 0.02% of F.S. |
Power | |
Max power per channel | 0.5 W |
Accuracy | ± 0.03% of F.S. |
Stability | ± 0.03% of F.S. |
Time | |
Current response time | ≤1ms(10% ~ 90% of F.S.) |
Charge and discharge conversion time | ≤20ms |
Time range of work step | (365 * 24) hours / work step Supported in time format: 00:00:00:00 (h, min, s, ms) |
● Voltage & Current Accuracy:±0.05% F.S.
● Sampling Time:100ms
● Number of Channels:16CH
● Temperature Range & Deviation:32℉ ~ 140℉±3.6℉(15℃ ~ 60℃±2.0℃)
● Heating Efficiency:77℉ ~ 140℉≤50min(25℃ ~ 60℃)
● Cooling Efficiency:77℉ ~ 59℉≤60min(25℃~15 ℃)
● Voltage & Current Accuracy:±0.01% F.S.
● Recording Frequency:100Hz
● Number of Channels:160CH
● Temperature Range & Deviation:32℉ ~ 140℉±3.6℉(0℃ ~ 60℃±2.0℃)
● Heating Efficiency:77℉ ~ 140℉ ≤30min(25℃ ~ 60℃)
● Cooling Efficiency:77℉ ~ 32℉≤50min(25℃~0 ℃)
● Voltage & Current Accuracy:±0.05% F.S.
● Sampling Time:100ms
● Number of Channels:64CH
● Temperature Range & Deviation:59℉ ~ 140℉±3.6℉(15℃ ~ 60℃±2.0℃)
● Heating Efficiency:77℉ ~ 140℉≤50min(25℃ ~ 60℃)
● Cooling Efficiency:77℉ ~ 59℉≤60min(25℃~15 ℃)
● Temperature Range :32℉~140℉(0℃~60℃)
● Ambient Air Temperature :41℉~86℉(5℃~30℃)
● Temperature Fluctuation:≤1.8℉(1℃)(No load and stable temperature)
● Cooling Efficiency:≤40MINS(77℉→32℉)(25℃→0℃)
● Heating Efficiency:≤30MINS(77℉→140℉)(0℃→60℃)
● Temperature Deviation:±3.6℉(±2.0℃)(No load and stable temperature)